| [36] Making a Chasing or forming tool |
We are assuming you are using W1 water hardening square stock drill rod, W1 tool steel. Many suppliers will sell W1 tool steel. It is often called drill rod (In England 'silver steel'). It should be square for less work in tool making, but round drill rod can be filed or forged to square. You should not use key stock, which some hardware suppliers will try and sell to you: it cannot be hardened as described below.... (2002)
 Complete Story |
| Show me more articles from: [Brain Press Publications]|[Charles Lewton-Brain] |
| Releated Categories:[Homemade Tools]|[Chasing and repousse] |
|
| [1019] Making a Heistad Cup in Three Minutes |
Fold-forming is a hand-working technique applied to single sheets of metal to create surfaces and three-dimensional forms quickly without soldering. It relies on the metal´s plasticity and ductility to make hundreds of complex forms resembling chased, constructed, and soldered shapes. Using thin materials, you can create light, volumetric objects and surfaces. Radical changes in cross-section are possible in only three to five minutes using simple tools such as a hammer, mallet, anvil, vise, rolling mill, and your fingers.... (2012)
 Complete Story |
| Show me more articles from: [AJM]|[Charles Lewton-Brain] |
| Releated Categories:[Step-by-Step Projects]|[Fold Forming] |
|
| [23] Making a pair of prong notching pliers |
These pliers notch round prongs easily to a given depth and replace a bur for the job. They are made to suit a specific size prong and one makes similar pliers for different prong shapes, but all based on this idea. One obtains a pair of chain nose pliers either new or from a flea market and converts them into prong notching pliers.... (1994)
 Complete Story |
| Show me more articles from: [Cheap Thrills in the Tool Shop]|[Charles Lewton-Brain] |
| Releated Categories:[Small Tools]|[Customize Your Tools] |
| ISBN: 096985106 |
| [984] Making a Riffle File |
Every now and then when you are fabricating a piece or polishing a casting, a hole or hollow will pop up that needs to be filed and smoothed. You can usually get at it using a bur and abrasive tools in your flex-shaft. But when you just can´t reach the hole, an old-fashioned tool called a riffle file comes in handy. Featuring various bent and curved shapes, these files fit into odd internal surface profiles. They were used extensively in the past for working on carved and chased steel dies intended for stamping out jewelry and other metal shapes. Years ago you could find dozens of curves and shapes, but today the tools are difficult to come by, so your best bet is to make your own.... (2011)
 Complete Story |
| Show me more articles from: [AJM]|[Charles Lewton-Brain] |
| Releated Categories:[Bench Tips & Tricks]|[Customize Your Tools] |
| ISBN: B00006K39S |
| [56] Making Earring posts by hand |
Yes you can make your own earring posts. It is generally more cost effective to buy them, but making them is not a problem and there are times that it is useful to know how.... (1997)
 Complete Story |
| Show me more articles from: [Brain Press Publications]|[Charles Lewton-Brain] |
| Releated Categories:[Wire Working]|[Hinges & Catches]|[Bench Tips & Tricks] |
|
|
|
|
|
| |
| |