There is a great way of doing very complex and repeated solderings in one go. This very important method uses casting and soldering investment is to set up multiple solderings at once. The idea is that you take clay (I prefer real clay, not plasticine - less oil and grease present to impede soldering) and make a 'bed' of it, a slab. Some people like to use a soft wax like 'BonBell' wax that covers small round cheeses instead of clay.... (2005) Complete Story
Extremely clean metal surfaces give better results. See the article on Cleaning metal Surfaces for more information on cleaning.... (1995) Complete Story
Making jewelry is sometimes seen as a difficult or an expensive proposition. In reality a basic metal working shop can be set up quite inexpensively. Cutting (separating materials), soldered construction and finishing are the three main things that jewellers do and what follows is a list of basic tools for doing these things. One should be able to set up a basic shop for less than a hundred dollars.... (1994) Complete Story
As well as being used for chasing they may also be used as punches to make textures. A stamp or texturing punch can be struck onto an annealed blank tool to get a negative impressions of its end. Each texturing tool can then produce its own negative. These blanks in turn are then hardened and tempered. It is wise to always wear goggles when using punches of any kind.... (1994) Complete Story
A good selection of burs may be had from your dentist. Dentists often throw out burrs which still have a reasonable life left in them for a jeweller. The same goes for the probes and other tools. Some dentists are nervous about giving tools away.... (1997) Complete Story
Would you like to reach Members of the Ganoksin Project to educate
them about the wonderful array of supplies, services and products
you have to offer?
Please request a copy of the Ganoksin Media Kit if you would like
more indepth information regarding Ganoksin's advertising services.