An alloy is by definition a mixture of two or more metals to create different strengths and colors. For granulation, the following formula is preferred. It is important to start with pure metals. Even trace amounts of impurities can result in flaws in the metal.... (2005) Complete Story
Here iss a nice little tool that makes use of an old setting bur. If you take the bottom teeth off a setting bur and polish the surface, you will have a tool that allows you to get right up next to the wall of a bezel and work on it without harming the metal on the bottom of the piece..... (2004) Complete Story
This is a great modification of pliers to give you a tool that mimics the shape of your thumb and forefinger meeting, but can get into places where your fingers are too large to go.... (2004) Complete Story