The Gem and Jewelry World's Foremost Resource on The Internet.
 
   for   in     
Add Ganoksin Power Search to your website
 
| Site Map | Jewelry Making Articles | Orchid Forums & Archives | Galleries | The BenchExchange | MetalCalc |
| Industry Web Sites Guide | Press Room | Advertising | Contact Us | Link to Us | More...

  Tips from The jeweler's bench
The Gem and Jewelry World's foremost Resource on The Internet. Open to the public, Free of Charge!
We are here to build a strong pool of information for the benefit of Web's jewelers and craftsmen - and those interested in jewelry and gemstones.
 
     
 
 
Advertise Here!
 
 
 
 

Back
Articles by Mark F. Grimwade
Page:
 
[377] Causes and Prevention of Defects in Wrought Alloys
Much of the recent literature on defects that occur in jewelry manufacture is focused on those occurring in lost wax investment casting, However, defects can also occur during casting of ingot and its fabrication into sheet, tube, wire and rod as well as their onward fabrication into jewelry components by processes such as stamping and forging. These defects, along with their causes and prevention, are briefly reviewed in this article.... (2002)
Complete Story

Show me more articles from: [The World Gold Council]|[Mark F. Grimwade]
Releated Categories:[Metals]|[Jewelry Mass Production]

 