The Gem and Jewelry World's Foremost Resource on The Internet.
 
   for   in     
Add Ganoksin Power Search to your website
 
| Site Map | Jewelry Making Articles | Orchid Forums & Archives | Galleries | The BenchExchange | MetalCalc |
| Industry Web Sites Guide | Press Room | Advertising | Contact Us | Link to Us | More...

If you benefit from what we're doing and want to give something in return, you can make a donation!

  Tips from The jeweler's bench
The Gem and Jewelry World's foremost Resource on The Internet. Open to the public, Free of Charge!
We are here to build a strong pool of information for the benefit of Web's jewelers and craftsmen - and those interested in jewelry and gemstones.
 
     
 
 
Advertise Here!
 
 
 
 

Back
Articles by Charles Lewton-Brain
Page: Previous  11 12 13 14 15 16 17 18 19 20  Next
 
[636] Fold Forming -T-Fold with a Table Insert
This page describes the steps to using a table insert in a T-fold. A table insert is an object, or a composition of a group of objects, inserted into the table when it is made, and then trapped. Items to try include, washers, shapes of 16 gauge iron binding wire, screws, shaped metal pieces designed for the purpose etc.... (2005)
Complete Story

Show me more articles from: [Brain Press Publications]|[Charles Lewton-Brain]
Releated Categories:[Fold Forming]

 

[398] Fold-Forming Rolled Fold: Heistad Cup
Rolled folds are folds which utilize the rolling mill and it's unique properties of equal, directional pressure on the plastic metal. Many pleated folds work well as do a series of flattened T-folds of various types. This one demonstrates the fold-forming priniciple of This rolled fold is called a Heistad Cup.... (2004)
Complete Story

Show me more articles from: [Brain Press Publications]|[Charles Lewton-Brain]
Releated Categories:[Fold Forming]

 

[475] Fold-Forming: Making a Basic T-fold
This article describes the steps to making a basic T-fold, one of the main categories of fold-forming. Numerous variations are possible from this simple starting place.... (2004)
Complete Story

Show me more articles from: [Brain Press Publications]|[Charles Lewton-Brain]
Releated Categories:[Fold Forming]

 

[826] Fold-Forming: Rolled Fold Procedures, Plunkett Fold
One of the most intriguing, and fastest ways to make fold-forms are in the Rolled fold part of the system. Rolled folds use the special, even pressure of the rolling mill to work the metal. They are either a package folded up and put through the mill like a Heistad Cup or are set up so that one side of the fold has more layers than the other when it is put through the mill. These travel further than the side with less layers when rolled, and, restrained by them, the whole fold curves as a result. This page describes the steps to making a Plunkett fold. The Good fold is derived from a Plunkett fold. These kinds of folds work well when forged as well as in the mill.... (2006)
Complete Story

Show me more articles from: [Brain Press Publications]|[Charles Lewton-Brain]
Releated Categories:[Fold Forming]

 

[670] Fold-Forming: T-Fold Boat Fold
The boat fold branch of T-folds is an interesting avenue. It permits you to have a curving, concave table, and to produce shaped tables as well as other complex derivations. The basic boat is begun by making a wedge T-fold. After the first angle is made the loop is tipped inthe other direction and pinched again to produce the boat pillow form.... (2005)
Complete Story

Show me more articles from: [Brain Press Publications]|[Charles Lewton-Brain]
Releated Categories:[Fold Forming]

 

Page Previous  11 12 13 14 15 16 17 18 19 20  Next