The Gem and Jewelry World's Foremost Resource on The Internet.
 
   for   in     
Add Ganoksin Power Search to your website
 
| Site Map | Jewelry Making Articles | Orchid Forums & Archives | Galleries | The BenchExchange | MetalCalc |
| Industry Web Sites Guide | Press Room | Advertising | Contact Us | Link to Us | More...

If you benefit from what we're doing and want to give something in return, you can make a donation!

  Tips from The jeweler's bench
The Gem and Jewelry World's foremost Resource on The Internet. Open to the public, Free of Charge!
We are here to build a strong pool of information for the benefit of Web's jewelers and craftsmen - and those interested in jewelry and gemstones.
 
     
 
 
Advertise Here!
 
 
 
 

Back
Articles by Charles Lewton-Brain
Page: 2 3 4 5 6 7 8 9 10  Next
 
[171] A jewelry workshop safety report: Safety and Substitutes
This talk briefly reviews issues of studio safety and discusses ways of recognizing risks in the studio and reducing hazard by substitution of materials or processes. The premise is that any reduction in risk improves the safety conditions of the goldsmith and artist. This approach to safety is practiced officially in European countries but is fairly new to North America. This paper today can only touch on things, be a skim, a snapshot. It is in fact a work in progress. The subject is a gigantic one, it feels rather like climbing a mountain where when you crest what appears to be the top of the rise there is yet another peak in front of one. This paper therefore skips and minimizes many important details. The book we are working on will address things in more depth.... (1998)
Complete Story

Show me more articles from: [The Jewelry Workshop Safety Report]|[Charles Lewton-Brain]
Releated Categories:[Workshop Safety]
ISBN: 0969851049

 

[195] A Method of Patinating Brass Alloys Using Contact Plating
This procedure should be undertaken with appropriate precautions; goggles, gloves, protective clothing, adequate ventilation. Recently I have been presented with the problems of repairing or changing the color of Indian made polished brass objects, usually to brown or grey tones. In one case the object was a Shiva which was about three feet high and across.... (1990)
Complete Story

Show me more articles from: [Brain Press Publications]|[Charles Lewton-Brain]
Releated Categories:[Patination]

 

[69] A method of patinating steel
As part of a large scale patination project in which I patinated a steel roof surface 24 by 48 feet on both sides I performed some 40 experiments to find out how to patinate the steel which was a requirement for structural reasons. In doing so I also experimented with paint.... (1990)
Complete Story

Show me more articles from: [Brain Press Publications]|[Charles Lewton-Brain]
Releated Categories:[Patination]

 

[164] A selected Jewelry / Metals Bibliography
A selected bibliography list for the jeweler - Metal working, Casting, Plating, Enamelling ,Gem Cutting, Setting, Engraving and Etching, Other Techniques, Jewelry Repairs and A Selected Bibliography for Materials Science for Goldsmiths - Over 100 listings.... (1997)
Complete Story

Show me more articles from: [Brain Press Publications]|[Charles Lewton-Brain]
Releated Categories:[Book reviews]

 

[68] An example of a paper die: after David Walker's version
The annealed metal is placed in a sandwich between soft 'pusher' paper and a hard paper which will serve as a monoprint paper die to emboss the metal sheet. The metal may be pre-polished.... (1990)
Complete Story

Show me more articles from: [Brain Press Publications]|[Charles Lewton-Brain]
Releated Categories:[Fabrication]|[Surface Manipulation]

 

Page 2 3 4 5 6 7 8 9 10  Next