[871] 105 Jewelers Bench Comments
In late 2006 I put together a survey on the Jewelers bench to which many Orchidians and others responded. There were a series of questions asked, and the answers were revealing, and contributed to my understanding of the jewelers bench and its functions, supporting my writing of the The Jewelers Bench, and MJSA/Orchid in Print book. Some of the specific answers were used in the book, but many served to buttress my arguments, or show me things I had not thought about. The answers were illuminating and, through their repetition of points they reinforced certain themes that are universal, and vital to the working jeweler and goldsmith. This article is then a compilation of these comments.... (2008)
Complete Story

Show me more articles from: [Ganoksin]|[Charles Lewton-Brain]
Releated Categories:[My Studio]

 

[899] 105 Jewelers Bench Comments
In late 2006 I put together a survey on the Jewelers bench to which many Orchidians and others responded. There were a series of questions asked, and the answers were revealing, and contributed to my understanding of the jewelers bench and its functions, supporting my writing of the "The Jewelers Bench", and MJSA/Orchid in Print book. In my teaching I will often ask students what they would tell a hypothetical friend, what is important to know, say about soldering and constructing a catch. What would you say that is important to keep your friend out of trouble and to ease their path? This then is the sense of the question addressed here about the jewelers bench.... (2009)
Complete Story

Show me more articles from: [Ganoksin]|[Charles Lewton-Brain]
Releated Categories:[My Studio]|[Beginner's Corner]

 

[171] A jewelry workshop safety report: Safety and Substitutes
This talk briefly reviews issues of studio safety and discusses ways of recognizing risks in the studio and reducing hazard by substitution of materials or processes. The premise is that any reduction in risk improves the safety conditions of the goldsmith and artist. This approach to safety is practiced officially in European countries but is fairly new to North America. This paper today can only touch on things, be a skim, a snapshot. It is in fact a work in progress. The subject is a gigantic one, it feels rather like climbing a mountain where when you crest what appears to be the top of the rise there is yet another peak in front of one. This paper therefore skips and minimizes many important details. The book we are working on will address things in more depth.... (1998)
Complete Story

Show me more articles from: [The Jewelry Workshop Safety Report]|[Charles Lewton-Brain]
Releated Categories:[Workshop Safety]
ISBN: 0969851049

 

[195] A Method of Patinating Brass Alloys Using Contact Plating
This procedure should be undertaken with appropriate precautions; goggles, gloves, protective clothing, adequate ventilation. Recently I have been presented with the problems of repairing or changing the color of Indian made polished brass objects, usually to brown or grey tones. In one case the object was a Shiva which was about three feet high and across.... (1990)
Complete Story

Show me more articles from: [Brain Press Publications]|[Charles Lewton-Brain]
Releated Categories:[Patination]

 

[69] A method of patinating steel
As part of a large scale patination project in which I patinated a steel roof surface 24 by 48 feet on both sides I performed some 40 experiments to find out how to patinate the steel which was a requirement for structural reasons. In doing so I also experimented with paint.... (1990)
Complete Story

Show me more articles from: [Brain Press Publications]|[Charles Lewton-Brain]
Releated Categories:[Patination]

 