[945] A Photo Tutorial on How To Make a Metal Leaf
A short while back I prepared this short photo tutorial showing how I make leaves from metal. I have use this method whenever shaping leaves that adorn my creations. The tools are minimal and the process is straight forward. The leaf shown was made from copper and I photographed the process in stages to show the simplicity of manufacture, which was less than an hour. I thought this may be of interest to someone who may be interested in making leaves.... (2011)
Complete Story

Show me more articles from: [Ganoksin]|[James Miller]
Releated Categories:[Fabrication]|[Step-by-Step Projects]

 

Page
 


 
Donate! If you believe in what we're doing, you can help!