The gemstone industry tends, for marketing reasons, to limit the definition of chalcedony somewhat more than mieralolgists. Among gemstone and jewelry sellers, the term chalcedony is usually used to refer specifically to semitransparent to translucent white, blue, pale grayish-blue, purple, pink, yellow, orange, red, or solid-colored materials other than carnelian, sard, or chrysoprase.... (2003) Complete Story