Hammers are an essential part of silversmithing and goldsmithing. While one can buy hammers ready made one can also do a lot with home-made versions and adaptations. Ordinary hammer heads may be reshaped providing they have not been cast. Reshaping....
(1994) Complete Story
Often craftspeople start out making craft objects in their living space, a kitchen, a living room, and sometimes continue working in them even when they have grown to the point that they need a separate studio. It is not wise to share one's living and family space with workshop space. Usually there are chemicals, tools, equipment, processes, sounds, materials, wastes, dusts and so on that are unhealthy to be exposed to that are produced in a work shop.... (2000) Complete Story
Hidden hinges are sometimes used on bracelets and jewelry pieces. I saw one on a Vietnamese bracelet once and have seen several on Diamonds International pieces. The place they pop up most frequently is in kitchen cabinets and doors on smooth surfaces like one sees on jet planes and sometimes on the sides of ships-hatches of various kinds. Look at these models because they are usually built to last and to be very sturdy. Kitchen cabinet hinges are a particularly fruitful resource.... (1996) Complete Story
A bearing is essentially tube sections which are attached to the metal being hinged into which the hinge itself is installed. The use of bearings offers us a couple of things. First of all, it offers us a way of increasing the structural strength of our hinge unit.... (1997) Complete Story
Not all sizes and wall thicknesses of tube come seamless from a factory or refiner. Especially when working in gold it is not cost effective or timely to order in a specific tube size, material, or wall thickness. There are many times when you need a piece of tubing, you don't have it, and you can't wait a day or so to order it in or run across town and buy it. In general, it is possible to make the length of tubing you require.... (1997) Complete Story