The original version of PMC was a bit tricky to solder, but PMC+ and PMC3 are both as dense as traditional metals, so soldering is just like working with traditional metals./nFrom: Quick Takes: PMC Basics by Tim McCreight DVD, 70 minutes, ISBN 1929565127/nby Tim McCreight© 2005 Brynmorgen Press

You need to have the Flash Player ver. 9.xx installed and a browser with JavaScript support.




URL
Embed
  Comments
Posted by platinumlake
(1086 days ago)
Thank you for the informative tutorial.
Posted by alacava
(1626 days ago)
Tried soldlering PMC years ago. It's wonderful to know
that I can do it now. Thanks for this tiny tutorial!

+ Flag : Feature This! - Innappropiate



Bookmark and Share Printer View Printer View
Donate! If you believe in what we're doing, you can help!