Rapid-Cast.com began selling Solidscape competitive Build and Support waxes in 2008.

Rapid-Cast Build material is stronger and more forgiving then our competitors build material, and yet burns out better then casting wax.  No residue or ash whatsoever.

Rapid-Cast Support material melts out at a lower temperature during post processing making clean up a breeze.

Both materials are less expensive then our competitor’s, with bulk pricing for large quantity, highly discounted orders.