From: Irisann Date: Thu Jul 29 19:43:50 1999 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Lori: Sorry to be remiss in answering your post but I had not gone into my e-mail for some days. You could try to get some hard silver (I think Rio Grande calls it "Spring-Finish") to use. I know that there have been pieces of silver floating around for decades with no harm to their clasps. If you have a kiln, you would also work harden it that way. The only thing that you might want to use the nickel silver for is the hinge-pin. If the clasp will rest against one's neck, I think it could cause allergies. Also, if you are going to make your own clasp, I would think it should be in silver so as not to cheapen the piece. Iris in Baltimore ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project