    I have to add my two cents to this one, soldering under water is
    hard if not down right impossiable. I used to do it all the time
    and it was just a pain in my south end. so here's what i came up
    with, and I have'nt lost a stone yet , knock on wood. I got some
    of that grain that they use in those rotating soldering trays
    and put just a touch of water in it, and I mean just a touch. I
    always had steam building up when i used water and it would blow
    out my little torch, a pisser at that. I bury the stone into
    this grain as far as I can with out covering up the spot I'm
    trying to solder. I order the replacement grain because it comes
    in a round can with a lid. It's about 6 inches or so around and
    an inch maybe an inch and a half high. It works great! I've
    soldered with emeralds and even turquiose, now it will depend on
    your skill and alot of luck , so you pays yer money and yous
    take yer chances at your own risk, but hey it's been working for
    me and it's alot easier than trying to do underwater soldering.
    I can give you a part no.#  and who I got it from if anyone's
    interested, just email me. 

Keep it shiny,  Matt the Catt
                                          


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project