========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== No offense to anyone but ditto on the daredevil wet finger method..... I use tissue paper soaked in water wrapped around the stone area. You can build up a tissue paper mache stand in a low walled can or ceramic dish. Immerse the protected section of the ring in water to insure that it doesn't dry out. Start with a lot of insulation and work down to to just enough to do the job, better too much that too little, all you'l be wasting is gas and clean and prep time if it doesn't go the first time. You will get a feel for the right amount. The trick is to cover enough of the ring to keep it cool, but not too much ; precluding adequate heat. A small but intense flame directed from the inside of the ring may help to keep it ftrom sputtering and messing the whole thing up, heat it up fast enough to flow the solder but not damage the stone or melt the gold. It's easier than it sounds, really! ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project