    Linda, When sizing rings that have heat sensitive stones, what I
    do is simailar to what has been suggested. my method is this..
    take an old crucible (round) fill it with real sand, say from a
    beach, put some water in the sand so that the sand is saturated.
    sink the top of the ring where the stones are into the wet sand
    and solder away. In the past 11 years I have never damaged a
    stone using this method. The metal will get hot but the sand and
    water will cool it enough to as to not effect the stone.. The wet
    paper towel method is useful BUT there is the risk of actually
    drying all the wetness up thus running the risk of cooking the
    stone.. you really need to watch what you are doing when using
    the paper towel method.. One very important thing to remember,
    when sizing a silver ring using any method, you will be using
    more heat for a longer time to get a proper solder joint, my
    suggestion is to go with the sand and water and you shouldn't
    have a problem. you will just need more patience.. When it comes
    to stones that can't take heat, the first thing I suggest is to
    take them out. I realize this is not always possible, that is
    when you should turn to the other methods.. Good luck.. feel free
    to ask anything any time... 

Marc Williams,  MarcCo. Jewelry Mfg.


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project