    Ray, Tom and Julie, 

    Thanks for your help. 

    A while ago, I tried to size a silver ring  (a 5mm or so band)
    with a green tourmaline and a CZ without removing the stones.  I
    used a heat shield product that is in a jar and a radioactive
    pink color.  The CZ crazed and the tourmaline blackened, so I
    threw out the pink stuff.   I now have an anthill garnet in a
    14K gold setting with a 7mm band that needs to be made smaller. 
    I have a "Little Torch", so 5 to 8 inch flames are not possible. 

    Would the pink stuff have worked if the ring were gold instead
    of silver?  I had also tried garnet sand quite some time ago,
    again with silver, but found it difficult to get solder to flow -
    too large a heat sink, I guess. 

    Are you really able to do the water thing with all kinds of
    stones?  I picture amethysts with citrine halos... 


Linda

 

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project