Sjartz Friday, July 09, 1999
   
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========


Vicki'
  Here's a short list of suppliers for you to try :

Thompson Enamel
catalog 
P.O. Box 310
Newport KY.
	41072
phone :606-291-3800
fax : 606-291-1849


Schlafers Enamel Supply
1012 Fair Oaks
So. Pasadena, Ca.
		91030
Phone : 818-441-1127

Bovano of Cheshire
Box 250
Cheshire, Conn.
1-800-847-3192

Enamelwork Supply Co.
1022 N.E. 68 th St.
Seattle, Wash.
98115
206-525-9271

Mandels Jewelry and Enamel Supply
P.O. Box 172
Startup, Wash.
98293
phone : 360-793-2807

American Metalcraft
2074 George St.
Melrose Park, IL.
60160-1515
phone : 708-345-1177
fax ; 708-345-5758
		
hope these help - good enameling !