========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== > Since it's come up about the toxicity of > Sparex.....does anyone know how long you can use the same batch > of Sparex G'day; Don't let's be miserly when using Sparex; it's so cheap to buy it as pool pH adjuster that you could easily afford to use a fresh batch every day; what; about 2c a pot? In any case if you don't want to 'waste' you might use the appearance of a pale blue colour in your pickle pot (the presence of copper sulphate) as an indication that it is about time to make up a fresh batch. Cheers, / \ / / / / / /__| \ johnb AT ts.co.nz (______ ) Mapua village is beautiful in spring. Which has thoroughly sprung. ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project