>            [snip]  that's why I always use a stoppered container,
>     usually one with a plastic lid and a glass body.Only a minor
>     amount of fumes seems to escape.  I haven't noticed any
>     appreciable rust forming for the 15-odd seconds that the jar is
>     open to retrieve the "soaking" item. 

    So you're taking the drill bits out by just soaking them cold in
    muriatic?  When I've tried that, it seemed to take forever...  I
    was talking about using it hot, just below boiling.  Plastic lids
    don't seem to stop the fumes then....  THEN it's fast, Buuttt... 
    So I use Alum, and I use it at a rapid boil.  Besides, our shop
    is across the street from a drug store, where I can pick up a
    little spice jar of alum if I happen to be out.  They don't have
    muriatic/HCL.  And, er. Well, I don't seem to have your stopperd
    containers so handy as one or another of those old beakers
    sitting by the sink which don't seem to have lids. Remember that
    normally when those drills break, I'm in a hurry, and just want
    to stick the ring in a beaker, put it on the hot plate, and be
    able to come back in a half hour and get on with the job... 

Peter

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project