Michele Stewart Sunday, June 24, 2012
   
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

>     There is no reason for this, silver copper and brass can all share
>     the same pickle with no issues. 

    So long as you don't introduce steel into the mix. Introducing steel
    to a saturated pickling solution creates an electrical charge. Just
    enough to copper plate any silver placed into it. Tres cool effect
    to see as anyone who accidentally used the wrong tongs to remove a
    piece from the pickle pot knows. 

Michele