Many of the pendants I have been getting have the crackle, and are
being called drusy's The process of causing the crackle interests
me, as does dying. You can not truly understand the market unless
you understand what humans are able to produce. There is a crackle
in the natural geode (thunder egg) process, it is pretty and it is
easy to dye. Chalcedony is the paler agate that is really easy to
dye because it is a greyish cream color. The dragon skin I bought
has ranged from blue, green, yellow, orange and a vibrant red. Done
well they are beautiful.
I just bought a drusy pendant that is black, with a strong band of
white and the bottom half looks just like an orange slice with the
membrane peeled back.
Would you like to reach Members of the Ganoksin Project to educate
them about the wonderful array of supplies, services and products
you have to offer?
Please request a copy of the Ganoksin Media Kit if you would like
more indepth information regarding Ganoksin's advertising services.