Hi Zed,
> anyone notice a yellowish hazy look on fused or fabricated
> argentium work?
When are you seeing this? Discoloration after heating, such as
annealing, soldering, fusing, or hardening is normal, and is removed
by pickling. Did you pickle after fusing? If this is happening
later, did you heat after polishing? Did you use a Goddard's Long
Shine Silver Cloth as a final polish? This cloth contains thiols,
which further retard tarnish.
Cynthia Eid
http://www.cynthiaeid.com