========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]========
Hi Folks..
> I drill hundreds of holes in the copper and am wondering if there
> are any recommendations that might help me get longer use or
> better use from my bits so that I can drill more pieces before
> having to throw away a dull bit.
With copper, make sure you're using brite (shiny) or TIN drills....
Gary W. Bourbonais