>     Is there a chart that indicates the length of metal I would
>     have to saw out for a particular ring size? And, should the length
>     be exact, or longer/shorter than denoted? 

    It's maths up to a point. Calculate the circumference from the
    diameter: it's a formula. You could make up a spread sheet and show
    each size in both dia and circumf. 

    But you must add a little extra for the physical effects of bending
    a strip of metal to a ring shape. People differ in their ways of
    calculating this, but a simple way would be to make the ring a
    little too small and stretch it up.

>     Is there a chart that would enable me to figure out total
>     surface weight without actually weighing something? For example, a
>     1 x 1 inch of whatever gauge sterling silver always weighs X grams. 

    It's also called density and specific gravity. Silver (fine) has a
    density of (approx) 10.5 grams per cubic centimetre. 

    Silver = 10.5 g/cm3
    Wax = 1 g/cm3 (approx)

    So take a 1" cube of wax and weigh it. That SAME SIZE would weigh
    10.5 times in silver. 

>     Are there any pitfalls I need to avoid when making a
>     ring/hollow ring? 

    Yes. Make a little hole for the acid pickle to exit out of. 

Brian
Auckland NEW ZEALAND
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project