>    This is a fairy tale created to justify stabilization of turquoise. 

    Tell me why the Aztecs oiled and waxed their turquoise, then? 

    And explain how, with the chemical/geological/gemological make-up of
    turquoise that it can be hard enough? It's very structure is porous
    in nature. 

    Turquoise that is that hard and non-porous is the fairy tale. I'm
    willing to suspend disbelief enough to say that there may be some
    VERY RARE pieces that have this quality, but I would also venture to
    say that no one on this list either has access to them or can afford
    them. And they were mined over 70 if not 100 years ago. 

    Sorry Leonid, on this one, you're wrong when it comes to anything
    that can realistically be obtained. And if you sell someone
    turquoise that you did not personally dig up and say that it's not
    stabilized, treated or altered, you're misleading your customers. 

Lindsay Legler
Dreaming Dragon Designs
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project