>     I have a client who is interested in purchasing a 1.00ct.
>     colorless cultured diamond 

    Currently the phrase "cultured" diamond is considered (by everyone
    except the synthetic diamond manufacturers themselves) to be
    misleading and unethical to use. The diamonds should be referred to
    as "synthetic diamonds". 

    It is very difficult for them to produce colorless diamonds, but
    according to some of their literature they are able to do this. I'm
    nor sure of their size range. The question is have you actually
    called and asked either Gemisis or Apollo and asked them directly?
    If they've said no they're not available to you then they aren't
    going to be available anywhere as these two companies are pretty much
    the leaders in the pack of synthetic diamond producers. 

Daniel R. Spirer, G.G.
Daniel R. Spirer Jewelers, LLC
1780 Massachusetts Ave.
Cambridge, MA 02140
www.spirerjewelers.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project