    I have found the kitchen timer to be great. When working I have many
    unique enamel projects going at once and group them for efficiency
    [enamel a group, grind a group, polish a group]. I bill by time so
    tracking is important. At this point I have 3 electronic timers that
    each can track 3 projects. I have put a small strip of frosted
    transparent tape by the #1, #2 and #3 timer buttons. I can then
    pencil in a descriptive word for each project [and erase when the
    project is done]. In this way it is a simple matter to just push the
    appropriate button when timing and keep a running tally on any
    project. 

    It is important to get a timer that will track up as well as down. I
    can tally that a job took 2 hours and 42 minutes - OR - set a timer
    for the 40 minutes it takes for my kiln to heat. 

    I have to add, if I am timing something important, like having to
    take something out of the pickle, I will use the clip on the timer to
    attach it to myself like a pager. It doesn't do any good if a timer
    goes off and you are away and can't hear it.........done that. 

Orchid Rules!
Karla in sunny S. California
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project