    Glass bead blasting is the best way to clean your gold and silver
    castings with out damaging it. 

    Two types of glass bead blasting can be used dry as well as wet. I
    am using wet bead blasting since 1992 for my gold and silver
    castings. 

    I prefer wet glass bead blasting since there is no dust generated
    and water provides a cushioning between the glass beads and casting
    surface and the cleaning is of surgical quality. The surface after
    wet bead blasting is clean surface which shows the defects in the
    castings if any clearly.So the wet or dry glass beads blasting can
    also be used as a quality control step. 

    I clean the wet glass beads regularly of the investment build up, so
    the casting surface remains shining and not mat.But Mat surface is
    some time good for some designs if no polishing is required. 

    Test your castings with wet as well as dry glass bead blasting, if
    the jewelery tools supplier provides this test before buying the wet
    or dry glass beads blaster. 

    Investing in a wet glass bead blaster will really prove beneficial
    in long run and you will be happy as I am. 

    May all be free of ill will, animosity, anger, hatred. 
    May all develop goodwill and love, peace and harmony. 
    May all be Happy and liberated. 

Umesh
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project