From: KARAT46 Date: Mon May 12 20:53:00 2008 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Peter Being one of the last US manufacturers of Titanium Solder Piks both the wooden handled and the Aluminum kind, I can tell you that you are right about Tungsten as it seems to last much longer than Titanium. It can be used at higher temperatures too for e,g Platinum. Another choice for the Professionals are tools with Ceramic tips. There are cross lock tweezers and probes available with Ceramic tips. Like the Diamond Tip Drills you really need the working ends of the tools to be of Good Titanium, Tungsten or Ceramic. If you see most of the picks are either wood handle or Alluminum. The Ceramic cross lock tweezers are made with regular stainless steel body. Then again it depends on the individual if you are going to use these all the time and also never loosing them they are worth paying more. That why we have BMW's, KIA's and now Smart cars. Regards Kenneth. Karat46 46 Jewelry supply New York. ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project