Re: [Orchid] Curing investment under pressure for casting  
  [Thread Prev] [Message Prev]      [Date Index]   [Thread Index]      [Message Next] [Thread Next]
From: John Donivan
Date: Sun May 04 03:02:15 2008
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

>     Might be wrong, but I believe the answer would be no. Water would,
>     at the least, be broken down to H and O. Probably more action.
>     Like being stripped of electrons or possibly forming into some sort
>     of plasma soup. 

    This has nothing to do with jewelry making, of course. And I'm not a
    black hole expert, either. But it's interesting.....First off, the
    SUN is plasma soup - peanuts. 

    To paraphrase the part of Einstein's Special Theory of Relativity
    that applies: 

    Space and time are actually one thing, called "spacetime", often
    called "The Space-time Continuum". An object in spacetime cannot
    exceed the speed of light, and also it must always move forward in
    time (so the theory goes). 

    Mass distorts the structure of spacetime. The presence of mass tends
    to tilt the direction of time towards the mass - not a definition of
    gravity, exactly, but we experience it as such. As you get nearer to
    a mass, time leans towards the mass (paraphrased). One object must
    move towards another because it is forward in time. As one nears an
    infinite mass, all time leads to the mass, and the effect is
    inexorable. Once you pass the "event horizon" (point of no return),
    you cannot excape the black hole because you cannot exceed the speed
    of light and you cannot go backwards in time. 

    The effect of all that is that (always remember this is all
    theoretical) what happens around a black hole has more to do with
    warping the very fabric of the universe than merely making plasma out
    of H2O or something like, "There's a lot of pressure in there." It's
    my thought, not necessarily science's, that it could be something
    like the reversal of the big bang. Everything around a black hole
    gets sucked inside, but the essential question is, where does it go
    and/or what does it become? These things are cutting edge physics and
    mathematics, and even string theory doesn't adequately address the
    questions... 

http://www.donivanandmaggiora.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project