    There are several good choices on small enameling kilns. The first
    is an electric kiln which looks like a beehive. You are limited to
    very small items and the heating is pretty uniform if the metal
    cover is placed over the piece. With a kiln without a temperature
    controller, you need to use care not to over heat your enamels or
    melt your items. 

    Next you have the microwave kiln you asked about. These actually
    come in a couple sizes. They take from 2 1/2 minutes to around 5
    minutes in a microwave oven, depending on the strength of the oven.
    Do be careful taking these in and out of your microwave as the top
    glory hole has a tremendous amount of heat comming from it. Moving
    these in and out of a microwave should be done with care as the
    interior of the kiln is extremely hot. That said they work very well
    for small projects. 

    The next option is either a PMC or small enameling kiln. Some have
    programmers built in, and regulate the temperature of the kiln and
    the melting enamel very accurately. These run from $570 - $630.00
    USD for the small kilns. The advantage with these is you can do
    small pendants and rings up to small bowls and light switch cover
    sizes. They offer a lot more versatility and at an affordable price
    can also be used for PMC. 

Best regards,
Phillip Scott G.G.

Technical Support
Rio Grande
1-800-545-6566
technicalsupport AT tbg.riogrande.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project