    I'm going a little nuts right now making custom child silhouettes.
    Most are brushed finish, but a few customers like a polished piece.
    The pieces are about 1" x 1" and flat, out of sterling silver. My
    problem is that I'll do thorough surface prep, sand to 1500 grit,
    then prepolish and polish. Everything is good to that point and I get
    a nice shine. Then I try and clean any compound off of the piece with
    a polishing cloth (2 piece rouge/polishing, or sunsheen cloth, as
    received, clean and new) or paper towel, or piece of clean flannel
    and immmediately it seems as if I'm putting horrible little fine
    scratches into the piece. 

    So my question is, what material/cloth/paper/etc should I use to do
    final cleaning of a piece? Is it possible that everything I own is
    contaminated with grit (If you've seen my house, the answer is
    probably yes)? How do you guys clean off the piece after polishing,
    removing fingerprints, etc? 

Thanks,
Nick
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project