Hello Cecile,

    So far as cleaning a delicate piece of jewelry made of wired silver
    and freshwater pearls, I use a dry vibratory tumbler with
    rouge-charged walnut shell (medium coarse size). The pearl surface is
    delicate, so I set a timer for 15 minutes and check on progress.
    Usually, things are bright enough, but if not, set the timer and
    tumble for another 5 - 10 minutes. 

    If the silver is quite tarnished, first do the washing soda (or
    baking soda will also work, just more slowly) in hot water and
    aluminum foil trick. An ionic cleaner will also remove tarnish well. 

    Then use the dry tumbler to bring back a polish. 

    Hope this helps - you're welcome to email offline. Judy in Kansas
    where it's a Seattle kind of day; misty and cool. Plants are loving
    it and the forsythia has really come out into bloom. Soon my turtles
    will be up, as will the asparagus and morels.
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project