Todd,

    A spindle with less runout will certainly help with the fuzzies but
    it's only part of the equation. I'd measure the runout on your
    current spindle so you can compare with others. 

    Here's some other suggestions that'll help eliminate them: 

    Make sure your stepover isn't too large for your cutter size. 

    Some people run a second pass, I don't find it necessary just to get
    rid of fuzzies. Sometimes, I'll run a second at 90 degrees to the
    first if I want a perfectly smooth surface. 

    Make sure you're using a good cutter, I had a few once that had
    terrible runout themselves. 

    Green wax has the most plastic and produces the toughest fuzzies, go
    ahead and give it a try if you'd like, but purple should be fine. 

    Use lube; a water based cutting fluid helps reduce them, I use a
    drip system, some people use a few drops of mineral or soy oil on
    the wax before cutting. 

    Give that master blaster a try again, I use a similar gun and it'll
    give me perfectly clean waxes. 

    These topics have all been covered in depth at 3dcadjewelry.com if
    you need more info or pics. 

Harry
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project