========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== I agree with Steph here, but want to add that since most GF is 14kt, use 14kt solder even 10kt will do in a pinch or if the color is more close to that of the lower karat plumb solder Vermeil, being 22-24kt over 999 silver -though far less actual gold with far less permanence -actually yields a better end result if one uses yellow silver solder (Hoover& Strong, Rio Grande, Contenti, etc) as opposed to 22-24kt, or any gold solder as the micronic coating of gold will melt into the silver before the melt or flow temperqture of plumb solder is reached. rer ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project