Hi,

    When buying a torch, consider the type of work you'll be using it
    on. You need a torch that will put out the quantity of heat (btu's)
    as well as the temp of the heat required by the metal being
    soldered/fused. 

    Without a doubt an hydrogen/oxy torch puts out a high temp flame.
    However, most water torches don't put out a flame with a high btu
    content (amount of of heat). Solder/fusing silver or copper over
    about 1" square generally requires more heat than these torches can
    provide. Working with this type/size of metal requires a higher btu
    content, the type put out by an acetylene/air or an acetylene/oxy
    torch with the appropriate size tip. 

    If you're going to be soldeing/fusing gold or silver in smaller
    pieces an acetylene/air or a butane fueled torch will probably work.
    If you plan to work on platinum you need a torch capable of a high
    temp. However, platinum can be contaminated with the carbon in a
    poorly adjusted torch using acetylene/oxy. The water torch may be
    satisfactory for platinum, unless you plan to use it to melt
    platinum for casting. Then it won't be capable of providing enough
    btu's, but the temp will be high enough. 

Dave
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project