Dear Hans,

    Funny you should ask! The issue "what IS enamel?" came up at our
    board meeting for the national Enamelists Society last weekend, in
    response to the proliferation of non-vitreous "enamel" fakes. Real
    Enamels are vitreous (glass). Enamel must be fired in a kiln or
    melted with a torch in order to form a sheet of glass and adhere to
    metal or other glass. I believe that most vitreous enamels will work
    well on either gold or silver (however, I primarily fire onto copper
    and then set in precious metals so take my advice with a grain of
    salt) 

    The Enamelists Society is a national organization for and about
    enamel and enamelists. The website provides a lot of information
    including resource lists, classes and workshops, local guilds, links
    to artists and more. Check it out! 

Marianne Hunter
http://www.hunter-studios.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project