Megan,

    Please understand that rubber and urethane are very different
    materials. There are 1000's of types of rubber, and 1000's of
    different formulations of urethane. Each formulation is designed for
    a specific purpose. The formulation we recommend for hydraulic
    forming has properties that allow it to form metals much more
    accurately and consistently with better longevity than other 'stock'
    formulations of urethane. 

    You can buy 'stock' grades from MSC (mscdirect.com) or other
    suppliers, you will be saving a little money now but it will cost you
    more in the long run. "Stock" formulations do not hold up as well and
    you'll be replacing your urethane more often. You will also get
    varied results with the pieces that you form with 'stock' urethane. 

    I am still using urethane I bought over 15 years ago. I also know of
    a University that purchased a great deal of "stock" urethane which
    failed by the end of a one week class. 

    I would highly recommend that you take a class from a qualified
    hydraulic forming instructor. You will gain a vast amount of
    knowledge about urethanes and techniques with regards to hydraulic
    forming. 

Sincerely,
Phil
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project