    Back in the days when my friend would my tubing on the band saw, the
    edges were very rough. I got a bottle of Nitric acid and I used a 1:5
    mix with water to eat the the edges smooth. Do this outside and not
    under any greenery that you value. The fumes are BAD and I noticed
    that tree leaves would brown and die after I did tubes under them.
    I'm sure that it's bad for the enviroment, but, I can't ever see that
    it would add a lot to the already existing pollutants. The acid also
    cleans the tubing so it will take the enamel well. You might be able
    to tumble the tubing with a good cut down medium. I intend to get one
    of those saws, myself, very soon. It may be summer before I can do
    much. In May and June we have 6 shows in 8 weeks. I'm going to be
    busy just keeping up, I hope. Cairenn, the Howling Artist
    www.howlingartist.com 

One is only as small as one's heart
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project