Hi everyone,  

    I am a woodworker and make wood jewelry. I make Ebony bracelets that
    I would like to add silver to the inner circumference of the bangle.
    These bangles have a flat inside with a small radius on each inside
    edge. They are 17 to 25 mm wide 

    I was thinking I could roll the silver up the radius to secure it. I
    work with wood tools, so my methods might seem a bit odd. 

    My idea is to create the lining by soldering a strip of silver 2 mm
    wider then the width of the bracelet. I would then slide the lining
    in the bracelet and put it on the lathe. I would spin the silver and
    roll it over. 

    I have read "Goldsmithing & Silver Work: Jewelry, Vessels &
    Ornaments" By Carles Codina. 

    I have never worked with silver in this way and wonder if anyone has
    any suggestions for rpm etc. 

Thanks
Mark Noll
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project