    First, THANK YOU ALL for participating in this excellent forum - I
    have learned so much, and I love to feel the connection with other
    craftspersons and artists. Although I've been reading a while, this
    is my first post (hope it goes where it's supposed to.) 

    My teacher told me to make some "super pickle" to clean up some
    intense oxidation - she said to use 1 T of Sparex to one cup hydrogen
    peroxide. This resulted in a thick white layer on the sheet of
    silver. When I showed it to her, she laughed and said, "no, 1 T of
    PICKLE (already mixed) and 1 c. hydrogen peroxide." So now I have
    this super, super pickle - can I use it for anything, and HOW do I
    get rid of it? It is a blue color - soaking silver and copper in it
    results in lots of small magnetized filings - I think it's the
    silver breaking down. It also stripped the enamel off my kitchen
    sink. Any ideas ? - (and yes, I CAN hear you laughing!) :) 

Thanks -
Sam Kaffine
Sterling Bliss
www.sterlingbliss.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project