    Hi....I have been corresponding with Beth - now will include you
    all....Ref the Citric Acid 

    I obtained a one pound sack of granules from Vitamin Cottage. Any
    Health Food Store ought to have it. I did transfer it with the label
    to a glass jar to keep it dry. 

    The proportion I experimented with this past weekend - 1 1/2 cup
    Citric Acid TO 1+ quart of water. It was heated on medium in the
    crockpot. Worked better when hot. There was no sign of an odor. As
    mentioned, always remember AW Acid to Water. 

    I also will try the PHDown - Beth I couldn't remember the name when
    I wrote. I got a bottle of liquid at Home Depot. There is PH Down for
    the Lily Pond as well as the Swimming Pool! Look for the Swimming
    Pool stuff. 

    The Orchid tips have really brought a lot of great ideas my way.
    Thanks for all the info. 

Rose Marie in Denver
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project