From: bill wismar Date: Wed Mar 12 23:12:30 2008 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== I usually use the plat/ir for most of my plat work even on plat/ru rings, most of the time it seems to work better for me. Don't know what laser you have but stuller has a great blog site for laser owners. If you use palladium get ready, it doesn't laser good, you can fill holes but so far I have not been able to laser anything that needs holding strength like prongs. Most of the wire that I use is 30 gauge. You are going to have a blast with the laser. Bill Wismar www.metalbendersgallery.com ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project