Re: [Orchid] Acidic environment in the studio  
  [Thread Prev] [Message Prev]      [Date Index]   [Thread Index]      [Message Next] [Thread Next]
From: John Burgess
Date: Wed Mar 12 23:03:38 2008
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

G'day - at your service, Judy!

    Barely volatile acid solutions in small amounts like sodium
    bisulphate at temperatures no higher than 30C should not cause much
    trouble in a reasonably sized area. If you use a warmed pickle, keep
    a lid on it always. 

    When I was well into jewellery (not done any for three years) I used
    only 10% sulphuric acid. But my jewellery bench is in the same very
    small room I used as a laboratory too, containing a variety of
    chemicals including acids, ammonia, etc. At the beginning I was
    worried about rusting of valuable tools (the room also contains a
    sink with H&C water and a very sensitive analytical chemical balance. 


    I gave all steel tools a coat of Turtle Wax car polish. And have had
    no bother with rusting. I also have a large wood lathe in the garage
    with about 25 big steel lathe tools - many made from old car springs.
    The lathe and all tools were treated with the wax too. I had to give
    up driving but that garage often contained a very wet car. No rust on
    any tool or the lathe. Now, it still contains the woodworking gear,
    plus a mobile clothes line - so we don't have to traipse out in the
    garden - plus my electric disability scooter. You may have to use the
    wax more often than I, but I'm a bit lazy! 

    I am not really any sort of expert these days: am past the use-by
    date at 86. But still read Orchid every day. My eyes are on the
    table, my teef are in a cup, my ears are in a drawer, my hands go on
    a walker frame, but still I won't give up! 

Cheers for now,
JohnB of NZ
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project