Hi Janet in Jerusalem,

>     A colleague of mine (many years of experience) said that it is
>     almost impossible to melt white gold solder a second time, and
>     consequently you can't really sweat solder with it. 

    I would not agree that you cannot flow white gold solder more than
    once, particularly easy white. Although I would agree that it's more
    difficult than other solders. Before the reheating of the solder the
    second time I would first pickle the piece (I use a citric acid
    pickle solution), then hang it in the ultrasonic and steam clean,
    then coat with boric acid and alcohol, heat with a soft flame until
    the boric acid has turned to a glaze, hit the hot seam with the
    solder with a squirt of batterns flux (I use a bottle with a
    syringe-like needle) and heat with that soft flame until it flows. 

    I know that sometimes you do everything right and it still won't
    flow. In that case I may add a little bit of solder to the seam to
    remind the solder inside what it's supposed to be doing. Hope that
    helps. 

Mark
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project