From: Daniel Culver Date: Thu Feb 21 20:05:31 2008 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== I haven't followed this whole thread, but what I do is; to maintain four pitch bowls I keep my pitch in a large slow cooker. Each bowl is kept full to within about three-quarter inch of the top. I use a ladle to add my pitch mix from a slow cooker (I used experience to find the setting were the pitch is just warm enough to spoon out) to the piece I working and if necessary to the bowl to support the piece. Since my pitch is formulated to be a little too soft ( talc and olive oil) to use at room temperate, I put the whole thing into the freezer for about 30 minutes while I work on another piece. Because I like the pitch soft formulated so I can develop fine detail faster in 18 gauge sterling, I can only work until the pitch softens further behind the thin layer next to the sterling that softenes quickly and when the metal starts moving too much or the whole piece starts moving from it's setting in the bowl it goes back into the freezer. I can't say this is the best way to work with pitch, but I like it. Working this way I sometimes use up to four bowls working for the day. Dan Daniel Culver ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project