From: Adams, Mitch
Date: Thu Feb 21 20:05:17 2008
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

>     there is a barrette by Stephen Walker, I'm interested in the
>     coloring of the red and rich yellow/gold tone. I think that is the
>     copper and brass which has been patinaed 

    Sorry I am late in answering. I am not Steve Walker, but I took an
    excellent workshop from him at Peter's Valley on Mokume and Married
    Metals two years ago. Steve likes to use heat to make his patina - no
    chemicals. The bright reds are from copper. Steve taught us to clean
    the metal completely and put it into a clean toaster oven that was
    preheated to 400 degrees F. Watch it carefully and pull it out when
    you hit the shades you want. All sorts of other colors can also be
    obtained depending on the heat, time in the oven, and alloy. The
    toaster oven produces a more even heat than a torch and is cheap ($20
    or so at Target) Yes, the heat patina will not last forever, but take
    your pictures while the colors are at a peak and enjoy them for a
    while thereafter. Chemically created patina (such as salt and LOS) is
    not permanent either. (except for grey and black) 

Mitch Adams
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project