Richard,

    I do not know about gum arabic, copper carbonate, or black copper
    oxide. I have successfully granulated with fine silver and I followed
    a multi-step process similar to the one outlined by Ronda Coryell in
    her DVD The Art of Granulation. There are many processes to it so
    maybe you will find out more specifically what you need help on once
    you start doing it. I highly recommend Ronda's video. There is also a
    wonderful tutorial in the Orchid articles by Sandra Buchholz. The
    glue-flux mixture needed for fine silver is a specific proportion of
    hide glue, yellow flux and distilled water. Klyr-fire glue I have
    heard will also work, as well as other things. Granulating with gold
    is somewhat different. I really want to granulate with 22 K gold
    right now, the problem is, my life savings will only buy enough gold
    for half the granules I need! 

    I used a beehive, or trinket kiln and coated the backs of my pieces
    with yellow ochre. 

    Actually the latest pieces I forgot to coat with ochre, and it was
    more difficult to accomplish. I just realized later that I never
    coated them. The home page on my site has a picture the latest
    earrings. I just need advice on final finishing. A local jeweler
    friend sandblasted one of my pieces and it looks really cool.
    Otherwise, the flat shiny part looks slightly blemished and
    polishing techniques that usually work great can mess up the
    granules. 

OK have fun
Connie
www.papayani.com
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project