>     I thought is a bit wierd, the claim for instance for "identical
>     volume" did not seem to make any sense. 

    The identical volume makes perfect sense. As James Binnion says, we
    cannot compress matter (well not solid or liquid matter anyway - we
    can compress a gas obviously). The mass of the coin will be identical
    to the original mass and the volume of the coin will be identical to
    the original volume, and its density will remain the same, but its 3D
    dimensions will differ from the original. Calculate the volume ((pi x
    radius) squared x thickness) from the new dimensions and they'll be
    the same as the calculated volume of the coin to start with. The
    original quoted explanation of what remained the same an what was
    changed was not very well written. "The resulting quarter maintains
    the same mass, volume, and density, but the size is drastically
    reduced!". The size in one dimension (or two in the case of a circle)
    is reduced but the size in the 3rd dimension (its thickness) is
    increased, therefore maintaining the coin's mass, volume and density.

Helen
UK
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project